MRI: Acquisition of a Multimodal, MEMS-Based Nanoindenter for Fundamental and Applied Materials Research, Education, and Outreach
Final report due
28 October 2027
in 375 days · The award ends on 30 June 2027.
GrantClerk is a private service. We are not NSF or any government agency.
Dates this award owes
NSF emails you about this too.
- Decide about an extension2 Mar 2027in 135 days
award ending 2027-06-30 · Research.gov
- Extension request16 May 2027in 210 days
award ending 2027-06-30 · Research.gov
- No-cost extension notice20 Jun 2027in 245 days
award ending 2027-06-30 · Research.gov
- Final report due28 Oct 2027in 375 days
award ending 2027-06-30 · Research.gov
- Project outcomes report due28 Oct 2027in 375 days
award ending 2027-06-30 · Research.gov
- Award is closed out28 Oct 2027in 375 days
award ending 2027-06-30 · Research.gov
Annual report dates come from the budget period on your award notice. That date is not public, so it is not shown here.
How we got this date
- NSF lists this award's end date as 30 June 2027.
- NSF rules say the final report is due no later than 120 days after that.
- So the final report is due by 28 October 2027.
Get a note before each report date
Add this award to your desk. We email you before each date and keep the dates in one place.
Renews each year until you cancel. Cancel any time from your account.
Award card
- Award number
- 2509529
- Period of support
- 1 Jul 2026 – 30 Jun 2027
- Amount
- $600,678
- Awardee
- University of Texas at Austin, Austin, TX
- Program
- Special Initiatives
- Directorate
- ENG
Abstract
The development of novel materials hinges on establishing a fundamental understanding of the interrelationship between materials structure, properties, processing, and functional behavior. A critical step in achieving this lies in leveraging characterization tools, especially multifunctional instruments that have exceptional capabilities and include advanced analytical methods. This Major Research Instrumentation…
Is this right?
We copy this from the public NSF award record. Your award notice and NSF always win. If a date looks wrong, check Research.gov.
More awards at University of Texas at Austin
- Travel: NSF Student Travel Grant for 2026 Computational Complexity Conference (CCC)Award 2617460
- A National Conference to Build a K-12 Quantum Education Ecosystem and Advance the Quantum Workforce PipelineAward 2628651
- Conference: Special trimester on Mathematical Developments in Geophysical Fluid DynamicsAward 2545649
- GOALI: CDS&E: New Algorithms for Analysis of Intact Protein Electrospray Mass SpectraAward 2554984
- Student Support for International Solid Freeform Fabrication (SFF 2026) Symposium; Austin, Texas; 2-5 August 2026Award 2629936
- Conference: Partnering for Impact Through Industry and Community Connections in Environmental Engineering Research and EducationAward 2625381
- I-Corps: Translation Potential of an ambient-air femtosecond laser sintering process that enables rapid fabrication of high-density copper filmsAward 2628113
- A field emission scanning electron microscope for geoscience research and student trainingAward 2547377