NSF award 2511730 · SUNY at Binghamton
MRI: Track # 1 Acquisition of an Atomic Layer Deposition System for Research and Training at Binghamton University
Final report due
29 July 2029
in 1,015 days · The award ends on 31 March 2029.
GrantClerk is a private service. We are not NSF or any government agency.
Dates this award owes
NSF emails you about this too.
- Decide about an extension1 Dec 2028in 775 days
award ending 2029-03-31 · Research.gov
- Extension request14 Feb 2029in 850 days
award ending 2029-03-31 · Research.gov
- No-cost extension notice21 Mar 2029in 885 days
award ending 2029-03-31 · Research.gov
- Final report due29 Jul 2029in 1015 days
award ending 2029-03-31 · Research.gov
- Project outcomes report due29 Jul 2029in 1015 days
award ending 2029-03-31 · Research.gov
- Award is closed out29 Jul 2029in 1015 days
award ending 2029-03-31 · Research.gov
Annual report dates come from the budget period on your award notice. That date is not public, so it is not shown here.
How we got this date
- NSF lists this award's end date as 31 March 2029.
- NSF rules say the final report is due no later than 120 days after that.
- So the final report is due by 29 July 2029.
Get a note before each report date
Add this award to your desk. We email you before each date and keep the dates in one place.
Renews each year until you cancel. Cancel any time from your account.
Award card
- Award number
- 2511730
- Period of support
- 15 Apr 2026 – 31 Mar 2029
- Amount
- $805,036
- Awardee
- SUNY at Binghamton, Binghamton, NY
- Program
- Major Research Instrumentation
- Directorate
- ENG
Abstract
Non-Technical description: Digital devices like smartphones and computers increasingly require smaller, faster, and more reliable components. Atomic layer deposition (ALD) systems help develop these components by coating complex surfaces with ultra-thin, uniform layers, often just a few atoms thick. These coatings improve the performance, safety, and durability of these devices. The acquisition of the ALD system…
Is this right?
We copy this from the public NSF award record. Your award notice and NSF always win. If a date looks wrong, check Research.gov.
More awards at SUNY at Binghamton
- Understanding the Key to Unlocking Fast Li-ion Conduction in Fluoride-based Solid ElectrolytesAward 2602721
- I-Corps: Translation potential of an artificial intelligence (AI) system designed to automate sleep stage scoringAward 2627391
- I-Corps: Translation Potential of a Paper Sensor Platform for the Rapid Detection of Cancer and Viral BiomarkersAward 2627835
- Collaborative Research: Developing and Evaluating Assessments of Problem-Solving in Computer Adaptive Testing EnvironmentsAward 2529441
- Collaborative Research: Mechanisms of moisture-driven ice growth: a warm Miocene data-model comparisonAward 2503814
- RET SITE: Empowering Educators with Hands-On Microelectronics Research: Cultivating Engineering Pathways for Secondary StudentsAward 2501940
- CAS-MNP: From the mother to the offspring: nanoplastic transfer and toxicity in aquatic speciesAward 2527197
- Collaborative Research: Nonlinear Electromechanical Dynamics for Ultra-Sensitive Gas Detection and Autonomous ActuationAward 2608059